The performance of the steel after tempering St60-2

The performance of the steel after tempering St60-2



Quenching St60-2 steel after tempering performance depends on its internal microstructure; St60-2 steel microstructure and its chemical composition, quenching process and tempering process. With the increase of tempering temperature,St60-2 steel tensile strength decreased; Yield strength was slightly increased first and then decreased; Reduction of area and elongation continue to improve.

In order to obtain good comprehensive mechanical properties, alloy structural steel is often in three different tempering temperature range: ultra high strength steel in 200 ~ 200 ℃; Near the spring steel at 460 ℃; Quenched and tempered steel in 550 ~ 650 ℃ tempering.

Carbon and alloy tool steel with high hardness and high strength, tempering temperature does not exceed 200 ℃. When tempering with secondary hardening alloy structural steel, high speed steel and die steel are within the range of 500 ~ 650 ℃ tempering.


E-mail: service1@katalor.com
Web:www.katalor.com
TEL: 0086-21-61182423
Skype: becky li (live:f7577499a4ddd17d)
Whatsapp:+8615538304508

没有评论:

发表评论