A537 Class 3 low temperature tempering

A537 Class 3 low temperature tempering

A537 Class 3 in the 150 ~ 250 ℃ tempering.

The purpose is to keep the quenching A537 Class 3 high hardness and wear resistance, reduce the quenching residual stress and the brittle.

Tempered martensite after tempering, refers to the quenching martensite in low temperature tempering of the organization. Mechanical properties: 58-64 HRC, high hardness and wear resistance.

Scope of application: mainly used in all kinds of high carbon steel tools and cutters, measuring tools, moulds, rolling bearing, carburizing and hardening the surface of the parts, etc.